Silicone vs EPDM, Nitrile, FKM, Neoprene and PORON: When Silicone Is Not the Right Material
Doc No SIL-MAT-07 Rev 1.0 Updated 2026-09 Document Material Guide · Silicone vs Other Elastomers Classification Published · Engineering reference
Silicone materials guide · Honest comparison

Silicone vs EPDM, Nitrile, FKM, Neoprene and PORON: When Silicone Is Not the Right Material

Silicone earns its place on temperature span, weathering, compression-set retention, and regulatory availability. It loses on tear strength, abrasion, oil and fuel resistance, gas permeability, and price. This page sets silicone against the elastomers and foams H-O converts most often, names the cases where another material is the better engineering answer, and lists the selection mistakes that most often send a silicone part back to review.

Part of the Silicone Materials guide. Start at the hub page for the forms, the selection matrix and the material families; this page goes deep on one topic.

LocationConverted in Winsted, CT · Family-owned since 1971 · ISO 9001:2015 certified organization · APQP / PPAP support on contract
30-second read

Specify silicone for heat above about 120 °C, cold below −40 °C, UV and ozone exposure, long-term compression at heat, or a regulation that names it. Choose EPDM for outdoor and steam duty under 120 °C at lower cost, nitrile or FKM for oil and fuel, PORON® urethane for indoor low-force seals under 90 °C, and natural rubber for abrasion. Fluorosilicone is silicone’s sibling for fuel zones, not a general alternative. Skip to the quote form →

Silicone sponge, EPDM, neoprene, and polyurethane foam sheet samples fanned out for comparison
Silicone sponge (left) against EPDM sponge, neoprene sponge, and polyurethane foam. Similar to the touch; very different once temperature, ozone, or compression set enters the drawing.
Quick Answer

Silicone is not always the right gasket material. EPDM beats it for hot water and steam to 150 °C and for outdoor duty under about 120 °C at lower cost; nitrile and FKM beat it in oils and fuels; PORON® urethane seals at lower force with tighter tolerance indoors under 90 °C; natural rubber wins on tear and abrasion. Silicone wins on continuous temperature span (−60 to 200/230 °C for general grades), UV and ozone, compression-set retention at heat, and the breadth of FDA, medical, flame and low-outgassing grades.

Property values are quoted from the source manufacturer TDS or the cited standard, not from H-O testing. H-O converts sheet and roll silicone; ratings belong to the specific grade and a finished assembly earns its own rating at the system level.

When To Spec What
  • Indoor enclosure under 90 °C, thin flange: PORON® urethane
  • Outdoor gasket under 120 °C: closed-cell EPDM
  • Oil mist or fuel at room temperature: nitrile or FKM
How it works
  1. 1
    Send drawing
    Upload a DXF, STEP, or PDF, or describe the gasket, pad, or insulator and its environment. A sample part works too.
  2. 2
    Material review
    Engineering checks the candidate grade against the manufacturer TDS: closure force, compression set, service temperature, fluid exposure, flame or regulatory requirement, and adhesive compatibility.
  3. 3
    Prototype
    24-hour prototypes on in-house materials; otherwise samples typically ship in 3–5 business days for common die-cut configurations on materials we commonly convert. Made-to-order; MOQ varies by material and part.
  4. 4
    Production
    Standard production runs ship about 2 weeks after drawing approval, including kiss-cut-on-liner and laminated configurations. Expedited service available. Ongoing parts run with lot traceability and TDS records.
Honest comparison

When silicone is not the right material

Silicone earns its place on temperature span, weathering, compression-set retention, and regulatory availability. It loses on tear strength, abrasion, oil and fuel resistance, gas permeability, and price. An engineer who specifies silicone for a room-temperature indoor gasket that sees oil mist is paying more for a worse part. The table sets silicone against the elastomers and foams H-O converts most often.

Continuous service temperature ranges: silicone compared with other gasket elastomers and foams Horizontal bars from minus 120 to plus 260 degrees C. Silicone (VMQ) spans about minus 60 to plus 200 or 230 degrees C with phenyl grades to minus 115; fluorosilicone minus 73 to 177; FKM minus 26 to 205; EPDM minus 57 to 121 (to 150 in water and steam); nitrile minus 34 to 121; neoprene minus 51 to 107; polyurethane foam PORON minus 40 to 90 continuous; natural rubber minus 55 to 80. Values from the Parker O-Ring Handbook and manufacturer data sheets; grade-specific. CONTINUOUS SERVICE TEMPERATURE · TYPICAL RANGES BY ELASTOMER (GRADE-DEPENDENT) −120 °C−400100200260 °C Silicone (VMQ)phenyl grades−60 to 200/230 Fluorosilicone (FVMQ)−73 to 177 FKM (fluorocarbon)−26 to 205 EPDM−57 to 150 (204 in water/steam) Nitrile (NBR)−34 to 121 Neoprene (CR)−40 to 121 Cellular urethane (PORON®)−40 to 90 continuous (121 intermittent) Natural rubber≈ −55 to 80
Figure 5. Temperature is the argument for silicone; everything else in the table below is the argument against it. Ranges from the Parker O-Ring Handbook (elastomers) and Rogers PORON 4701-50 TDS (urethane); phenyl silicone to −115 °C and silicone to 232 °C are handbook values for special compounds, and every range is grade-specific. [63] [62]
MaterialWhere it beats siliconeWhere silicone beats itTypical H-O useCost tier (relative)
EPDM (sponge or solid)Hot water and steam to 150 °C; UV and ozone at lower cost; roughly double the tensile strength; the default for outdoor and HVAC gaskets under about 120 °CCompression set at heat (EPDM ≈35–48% vs silicone foam 2–5% in Rogers’ comparison); dry-heat ceiling; cold flexibility below −50 °C; regulatory rangeEnclosure, HVAC, fenestration, and construction gasketsLow
Nitrile (NBR)Petroleum oils and fuels; abrasion; low cost; wide durometer rangeEverything outdoors (NBR ozone-cracks), heat above 120 °C, cold below −34 °C, food-contact clarityOil-zone gaskets, fuel-resistant washers, cork-nitrile flange gasketsLow
FKM (fluorocarbon)Fuels, oils, aromatics, and heat to 205 °C in one polymer; lowest gas permeability of the groupLow-temperature flexibility (FKM stiffens near −26 °C); price (FKM is the only common gasket elastomer above silicone in cost); softness and conformabilityChemical-zone and high-temperature fuel sealsHighest
Neoprene (CR)Moderate oil resistance with toughness, flame retardance in some grades, low price; forgiving in dynamic and abrasive duty. H-O converts MIL-PRF-6855 Class 2 neoprene sheet (30 A, −67 to 220 °F) for military drawings that call it out.Heat above about 107 °C; compression set; UV over long exposure; cold below −50 °CGeneral industrial gaskets, vibration pads, protective stripsLow
Cellular urethane (PORON®)Lowest closure force at thin gauges; compression set ≤10% (D3574, 70 °C); tighter thickness tolerance; lower price than cast silicone foam; excellent for electronics cushioningContinuous temperature (PORON 4701-50: 90 °C continuous); UV and hydrolysis outdoors; water absorption when uncompressed; flame ratings (HBF vs V-0); high-temperature setDevice cushioning, indoor enclosure gaskets, EV pack compression pads at moderate temperatureMedium
Natural rubberHighest tear, tensile, and abrasion at the lowest cost; resilienceHeat, ozone, oil, weathering, and every regulatory categoryWear pads and dynamic parts onlyLowest
Fluorosilicone (FVMQ)Not an alternative but a sibling: fuel and oil resistance with silicone’s cold flexibilityPrice, tear, hot-air ceiling, compression set on sponge gradesAerospace fuel-zone and hydraulic-zone sealsHigh

Cost ranking (most to least expensive) across common gasket elastomers, per an industry converter’s comparison: FKM > silicone > urethane > nitrile > neoprene > EPDM > natural rubber. [64] Compression-set comparison values from the Rogers Technical Sealing Guide are on a D3574 basis and differ from the D1056 data-sheet figures for the same silicone foam. [5] H-O’s blog posts compare these choices for specific jobs: switchgear cabinet gaskets (EPDM vs silicone vs butyl), EV compression pads (PORON vs silicone foam), and EV module seals (silicone vs EPDM vs neoprene).

Three cases where another material is the better engineering answer

Indoor enclosure under 90 °C with a thin flange: PORON® urethane seals at lower force, holds a tighter thickness tolerance, and costs less. Outdoor HVAC or fenestration gasket under 120 °C: closed-cell EPDM weathers as well as silicone for a fraction of the price. Oil-mist or fuel exposure at room temperature: nitrile or FKM will outlast VMQ, and fluorosilicone is only the right choice when cold flexibility is also required.

What goes wrong at spec

Common silicone selection mistakes

Eleven patterns that come back from review, each with the correction that prevents it.

MistakeWhat happensCorrection
Specifying “silicone, 50 durometer” for a cellular gasketSupplier substitutes any sponge or foam; closure force and set are uncontrolledCall out form, grade or spec (ASTM D1056 line callout, AMS 3195/3196, or manufacturer grade), and CFD range
Treating “foam” and “sponge” as synonymsA 15–20% set sponge replaces a 2–5% set foam in a permanently compressed jointState compression set with method and condition on the drawing
Designing to the typical CFD instead of the spec rangeA lot at the top of the 6–14 psi range doubles the closure force of a lot at the bottomDesign to the range or ask for a tighter band; verify latch force at the upper bound
Using an intermittent temperature rating as continuousGasket hardens and loses recovery in monthsDesign to the continuous rating; request heat-aging data
Assuming any silicone is FDA, medical, or V-0Regulatory file fails audit; wrong color or cure shippedSpecify the grade, color, and the document that supports the claim
Applying an acrylic PSA to silicone without a planAdhesive releases from the silicone side in serviceUse a silicone PSA or a differential tape with the silicone side to the rubber; treat PSA as a mounting aid
Ignoring the adhesive’s temperature limitSilicone rated to 200 °C, acrylic PSA rated to 149 °C; bond fails firstSpecify a silicone PSA above about 150 °C, or mechanical retention
Choosing VMQ for a fuel-zone sealSwelling of 20–30% or more; extrusion and loss of sealFluorosilicone with immersion data in the actual fluid
Confusing thermal and electrical conductivityA gap pad specified where an EMI gasket was needed, or the reverseName the function and the test (D5470 vs D991 / MIL-DTL-83528)
Narrow lands and sharp inside corners in thin foamParts tear on the liner or at installationRadius corners; widen lands; consider a carrier or reinforced grade
Reading a metal-detectable test specimen as a line thresholdFragments below the plant’s actual sensitivity pass undetectedValidate on the plant’s detector with the plant’s product
Engineering FAQ

Questions engineers ask about this topic

Direct answers with the source. The same questions appear in the page’s structured data.

6 questions · click a question to expand its answer

Is fluorosilicone better than silicone?

Only where fuel, oil, or non-polar solvent contact is present. Fluorosilicone (FVMQ) swells under 5% in IRM 903 oil where general silicone swells 26–30% in one manufacturer’s comparison, and it keeps silicone’s cold flexibility (−73 °C class). It costs more, has a lower hot-air ceiling (about 175–200 °C), higher compression set in sponge form, and no advantage against water, steam, ketones, or brake fluid. For an indoor or outdoor gasket with no hydrocarbon exposure, VMQ is the better and cheaper choice. [6] [37]

Silicone vs EPDM: which is the better gasket material?

EPDM for outdoor, HVAC and steam duty under about 120 °C (to 150 °C in water and steam) at lower cost and roughly double the tensile strength. Silicone for dry heat above that, cold below −50 °C, long-term compression at temperature (EPDM sponge sets about 35–48% in Rogers’ comparison versus 2–5% for silicone foam), and where FDA, medical, flame or low-outgassing grades are required. Both resist UV and ozone. [5] [63]

Silicone vs neoprene: when does neoprene win?

When the gasket sees moderate oil, abrasion or dynamic handling at room-to-warm temperature and price matters. Neoprene (CR) is tougher and cheaper than silicone and tolerates moderate oil exposure; its limits are heat above about 107 °C, compression set, cold below about −50 °C, and long UV exposure. Silicone wins for heat, cold, long-term set, and every regulated application. [63]

Silicone foam vs PORON urethane: which for an enclosure gasket?

PORON® for indoor enclosures under 90 °C continuous: lower closure force at thin gauges, compression set ≤10% (D3574, 70 °C), tighter thickness tolerance and lower price. Silicone foam when the joint sees temperatures above that, UV or hydrolysis outdoors, a UL 94 V-0 requirement (PORON is typically HBF), or long-term set at heat. Both keep 45–75% of sealing force after 60 h in Rogers’ comparison, far better than EPDM or neoprene. [62] [5]

Silicone vs nitrile or FKM for oil and fuel?

General silicone (VMQ) swells badly in hydrocarbons (roughly 26–30% by volume in IRM 903 oil in one manufacturer comparison), so nitrile is the economical choice for oil at moderate temperature and FKM for fuel, oil and aromatics with heat to 205 °C. Choose fluorosilicone only when fuel resistance and cold flexibility are both required, as in aerospace fuel zones. Nitrile cannot be used outdoors (ozone cracking) and FKM stiffens near −26 °C. [63]

Is silicone more expensive than other gasket materials?

Usually. A directional industry ranking places FKM above silicone, then urethane, nitrile, neoprene, EPDM and natural rubber. Cast silicone foam also costs more per sheet than blown sponge in many grades. The premium is justified where temperature span, compression-set retention, weathering or a regulatory grade is required; for a room-temperature indoor gasket with no such driver, EPDM, neoprene or PORON® is the better-value part. [64]

Sources for technical claims

References

Every quantitative claim on this page traces to one of the sources below. Reference numbers are shared across all eight pages of the Silicone Materials guide so a value cited as [4] here is the same source as [4] on any other page. Values change between data-sheet revisions; the revision on file at publication governs.

Show all 6 sources cited on this page tap to expand
6 sources · click to expand, or expand all
Rogers Technical Sealing Guide (PORON® and BISCO®)

Stress relaxation mostly in first 1–2 h; silicone/PORON retain 45–75% of force at 60 h vs 15–35% for EPDM/neoprene; compression-set comparison at 70 °C and 100 °C (D3574 basis); water leakage vs width and compression at 1.5 psi; NEMA/IP mapping; UL 50E gasket test levels. rogerscorp.com (PDF)

Shin-Etsu silicone rubber performance data

Oil-swell comparison: general silicone +26–30% volume in IRM 903 (150 °C/70 h) vs fluorosilicone under 5%; fluorosilicone in Fuel C about +4%; compression-set and heat-aging ranges by grade. shinetsusilicone-global.com (PDF)

SSP: Understanding MIL-DTL-25988 fluorosilicone

Types I–IV (Type II sheet/roll), Classes 1–4, Grades 40–80 Shore A; continuous −55 to +175 °C, short-term to +200 °C. sspinc.com

Rogers PORON® 4701-50 data sheet

15/20/30 pcf; CFD 10–39 psi (D3574 C); compression set ≤10% (D3574 D, 70 °C); continuous 90 °C, intermittent 121 °C; 0.012–0.5 in. rogerscorp.com

Parker O-Ring Handbook (ORD 5700): elastomer temperature ranges

Silicone −115 to 232 °C (special compounds); fluorosilicone −73 to 177 °C; EPDM −57 to 150 °C (to 204 °C in water/steam); nitrile −34 to 100 °C (121 °C with shorter life); FKM −26 to 205 °C; neoprene (CR) −40 to 121 °C; polyurethane −40 to 82 °C. parker.com (PDF)

Gasket elastomer cost ranking (Canada Rubber Group)

Relative cost, most to least: FKM > silicone > urethane > nitrile > neoprene > EPDM > natural rubber > SBR. Directional only. canadarubbergroup.com

Engineering review

Need help selecting a silicone?

Send H-O your drawing, operating temperature, environment, compression requirements, regulatory requirements, adhesive needs, and expected quantity. Our team reviews the application against current manufacturer data and helps identify appropriate material constructions for prototyping and production. We typically respond within one business day.

Contact
Your application
Compression, part & quantity
Typical response in one business day. 24-hour prototypes on in-house materials; otherwise samples typically 3–5 business days; production in 2 weeks. MOQ varies by material and part. Expedited service available. Prefer the phone? Call (860) 469-1144.
Continue reading

See also: the rest of the Silicone Materials guide

The guide is one hub and seven topic pages that share one set of sources and one set of numbers.

Silicone materials guideSilicone Materials hubEngineering guide to silicone materials: solid rubber vs sponge vs foam, selection matrix and decision flow, specialty silicones, and the material families H-O converts, with TDS-cited data.Read the guideSilicone materials guideFoam vs sponge vs solidHow cast silicone foam, closed-cell silicone sponge and solid silicone sheet differ in structure, CFD, compression set, sealing and mechanical behavior, with grade data from Rogers, Silicone Engineering and Saint-Gobain.Read the guideSilicone materials guideProperties: CFD & compression setCompression force deflection vs compression set for silicone gaskets: test methods, formulas, a 14-material benchmark, a worked closure-force example, and 18 engineering properties explained by how they are used.Read the guideSilicone materials guideMetal-detectable siliconeMetal-detectable silicone rubber explained: why it exists, how in-line detection works, Silicone Engineering metectSil grades and test conditions, the H-O 40–85 Shore A detectable grade, solid vs sponge, FDA compliance, and converted gasket options.Read the guideSilicone materials guideSpecialty silicones & cure systemsFourteen specialty silicone families and the cure systems behind them: high-temperature, flame-retardant, low-outgassing, insulating, conductive, thermally conductive, fluorosilicone, medical, food-contact, antimicrobial, reinforced, high-tear, translucent and membrane grades, with what to evaluate and the design risk for each.Read the guideSilicone materials guideAdhesive-backed siliconeHow to put pressure-sensitive adhesive on silicone foam, sponge and solid gaskets: why acrylic fails on silicone, silicone PSA vs differential tape, peel and temperature data from 3M and Rogers, shelf life, and the mounting-aid rule.Read the guideEngineering toolRubber chemical compatibility chartFluid resistance by elastomer.Read the guideBlogSwitchgear cabinet gaskets: EPDM vs silicone vs butylA worked selection for one joint.Read the guide