POLYMER:
Natural Rubber
DENSITY (AVERAGE) [ASTM D1056]:
33 lb/ft3
COMPRESSION DEFLECTION @ 25% [ASTM D1056]:
16-22 psi
COMPRESSION DEFLECTION CHANGE AFTER OVEN AGING 168 HOURS @ 158°F [ASTM D1056]:
±20%
COMPRESSION SET @ 50% DEFLECTION @ 158°F [ASTM D1056]:
15%
TEMPERATURE RANGE:
-20°F to 160°F
ABRASION RESISTANCE:
Yes
CELL STRUCTURE:
Open Cell

- Technical Datasheet
- Permanent Adhesive - Silicone/Acrylic [APSADP], [SA1060

Product Overview

Firm, open cell natural rubber.

Typical Applications:
• Cushioning foam for applications where high firmness is required

Product Features & Benefits:
• Anti-slip and high coefficient of friction
• Extremely resistant to abrasion and tearing
• Can be laminated with a broad range of materials including textiles and cork
• Low compression set
• Quick compression recovery